Resources

In a materials science laboratory, four polished metal disks—Silver (Ag), Copper (Cu), Polished Aluminum (Al), and Lead (Pb)—are evaluated for electrical conductivity using a four-point collinear probe apparatus, and surface luster using a specular glossmeter at a 60∘60^\circ incident angle. The four-point probe delivers a current I=100.0 mAI = 100.0\text{ mA} and measures potential differences ΔV\Delta V across outer to inner pins on specimens of equal thickness t=1.00 mmt = 1.00\text{ mm} (sheet resistance formula Rs=πln⁡(2)ΔVIR_s = \frac{\pi}{\ln(2)} \frac{\Delta V}{I}, conductivity σ=1Rst\sigma = \frac{1}{R_s t}). Specimen 1 yields ΔV=0.350 μV\Delta V = 0.350\ \mu\text{V} and gloss value 95 GU95\text{ GU}; Specimen 2 yields ΔV=4.60 μV\Delta V = 4.60\ \mu\text{V} and rapidly develops a dull gray tarnish (22 GU22\text{ GU}); Specimen 3 yields ΔV=0.372 μV\Delta V = 0.372\ \mu\text{V} and gloss 90 GU90\text{ GU}. (a) Calculate the electrical conductivity σ\sigma for Specimen 1 and Specimen 2. (b) Correctly assign the identities of Ag, Cu, and Pb among Specimens 1, 2, and 3, and explain the chemical cause for the loss of luster in Specimen 2.

Answer and steps

Final answer

(a) Specimen 1: σ=6.30×107 Ω−1⋅m−1\sigma = 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}; Specimen 2: σ=4.80×106 Ω−1⋅m−1\sigma = 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}; (b) Specimen 1 is Silver (Ag), Specimen 2 is Lead (Pb), Specimen 3 is Copper (Cu); Lead loses its metallic luster because spontaneous surface oxidation forms an incoherent, non-metallic passivating oxide/carbonate film (PbO\text{PbO}/PbCO3\text{PbCO}_3) that scatters incident light diffusely instead of specularly.

Steps

01

Specimen 1

Part (a): Calculating Electrical Conductivity (σ\sigma)

The four-point probe method relates the sheet resistance RsR_s, specimen thickness tt, and bulk electrical conductivity σ\sigma via: Rs=πln⁡(2)⋅ΔVIR_s = \frac{\pi}{\ln(2)} \cdot \frac{\Delta V}{I} σ=1Rs⋅t=ln⁡(2)π⋅t⋅IΔV\sigma = \frac{1}{R_s \cdot t} = \frac{\ln(2)}{\pi \cdot t} \cdot \frac{I}{\Delta V} Given parameters:

  • Current: I=100.0 mA=0.1000 AI = 100.0\text{ mA} = 0.1000\text{ A}
  • Thickness: t=1.00 mm=1.00×10−3 mt = 1.00\text{ mm} = 1.00 \times 10^{-3}\text{ m}
  • Geometric constant factor: ln⁡(2)π⋅t=0.693153.14159⋅1.00×10−3 m≈220.64 m−1\frac{\ln(2)}{\pi \cdot t} = \frac{0.69315}{3.14159 \cdot 1.00 \times 10^{-3}\text{ m}} \approx 220.64\text{ m}^{-1}

Substitute ΔV=0.350 μV=3.50×10−7 V\Delta V = 0.350\ \mu\text{V} = 3.50 \times 10^{-7}\text{ V}:

σ1=220.64 m−1⋅0.1000 A3.50×10−7 V≈6.30×107 Ω−1⋅m−1\sigma_1 = 220.64\text{ m}^{-1} \cdot \frac{0.1000\text{ A}}{3.50 \times 10^{-7}\text{ V}} \approx 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}

02

Specimen 2

Substitute ΔV=4.60 μV=4.60×10−6 V\Delta V = 4.60\ \mu\text{V} = 4.60 \times 10^{-6}\text{ V}:

σ2=220.64 m−1⋅0.1000 A4.60×10−6 V≈4.80×106 Ω−1⋅m−1\sigma_2 = 220.64\text{ m}^{-1} \cdot \frac{0.1000\text{ A}}{4.60 \times 10^{-6}\text{ V}} \approx 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}


Part (b): Metal Assignment and Cause of Tarnishing

01

Assigning Metal Identities

Conductivity in metals is governed by the electron-sea model, depending on the density and mean free path of delocalized valence electrons. The intrinsic electrical conductivities of the metals follow the trend: σ(Ag)>σ(Cu)>σ(Al)>σ(Pb)\sigma(\ce{Ag}) > \sigma(\ce{Cu}) > \sigma(\ce{Al}) > \sigma(\ce{Pb})

  • Specimen 1 has the lowest measured voltage drop (ΔV=0.350 μV\Delta V = 0.350\ \mu\text{V}), giving the highest conductivity (σ≈6.30×107 Ω−1⋅m−1\sigma \approx 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}). This identifies Specimen 1 as Silver (Ag\ce{Ag}).
  • Specimen 3 has a slightly larger voltage drop (ΔV=0.372 μV\Delta V = 0.372\ \mu\text{V}), corresponding to σ≈5.93×107 Ω−1⋅m−1\sigma \approx 5.93 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}, which is characteristic of the second-most conductive metal, Copper (Cu\ce{Cu}).
  • Specimen 2 displays a much larger voltage drop (ΔV=4.60 μV\Delta V = 4.60\ \mu\text{V}), yielding a conductivity an order of magnitude lower (σ≈4.80×106 Ω−1⋅m−1\sigma \approx 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}). This corresponds to the post-transition metal Lead (Pb\ce{Pb}).
02

Chemical Mechanism for Loss of Luster in Specimen 2

  • Metallic Luster Mechanism: In clean metals, mobile conduction electrons absorb incident light frequencies and re-emit them in phase, creating high specular reflection (mirror-like gloss).
  • Tarnish Formation: Lead (Pb\ce{Pb}) reacts spontaneously with atmospheric OX2\ce{O2}, moisture, and COX2\ce{CO2}: 2Pb+OX2⟶2PbO2\ce{Pb} + \ce{O2} \longrightarrow 2\ce{PbO} PbO+COX2⟶PbCOX3\ce{PbO} + \ce{CO2} \longrightarrow \ce{PbCO3}
  • The resulting non-conductive, ionic/covalent layer of PbO\ce{PbO} and PbCOX3\ce{PbCO3} lacks the free electron density needed for specular reflection. Instead, its microcrystalline roughness causes diffuse light scattering, resulting in a rapid drop in measured gloss from a metallic sheen down to a dull gray tarnish (22 GU22\text{ GU}).

Typical errors

OverviewACEpath Teacher's Diagnosis

01 The student forgets to convert microvolts to volts, yielding conductivity values that are off by a factor of 10⁶.

Sample Student Work

Reviewed by ACEpath Teacher
Step-by-Step Review
Walk Through It with Your Teacher
Partially correct
  1. Step 1

    I=0.100 A, t=0.001 m  ⟹  σ=ln⁡(2)⋅Iπ⋅t⋅ΔVI = 0.100\text{ A},\ t = 0.001\text{ m} \implies \sigma = \frac{\ln(2) \cdot I}{\pi \cdot t \cdot \Delta V}

  2. Step 2

    σ1=ln⁡(2)⋅0.100π⋅0.001⋅0.350=63.0 S/m\sigma_1 = \frac{\ln(2) \cdot 0.100}{\pi \cdot 0.001 \cdot 0.350} = 63.0\text{ S/m}

    Correct

    σ1=ln⁡(2)⋅0.100 Aπ⋅(1.00×10−3 m)⋅(0.350×10−6 V)≈6.30×107 Ω−1⋅m−1\sigma_1 = \frac{\ln(2) \cdot 0.100\text{ A}}{\pi \cdot (1.00 \times 10^{-3}\text{ m}) \cdot (0.350 \times 10^{-6}\text{ V})} \approx 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}

    You substituted the voltage as 0.3500.350 rather than converting 0.350 μV0.350\ \mu\text{V} to 3.50×10−7 V3.50 \times 10^{-7}\text{ V}. Because microvolts were not converted to base SI units, your result is understated by a factor of 10610^6.

  3. Step 3

    σ2=ln⁡(2)⋅0.100π⋅0.001⋅4.60=4.80 S/m\sigma_2 = \frac{\ln(2) \cdot 0.100}{\pi \cdot 0.001 \cdot 4.60} = 4.80\text{ S/m}

    Correct

    σ2=ln⁡(2)⋅0.100 Aπ⋅(1.00×10−3 m)⋅(4.60×10−6 V)≈4.80×106 Ω−1⋅m−1\sigma_2 = \frac{\ln(2) \cdot 0.100\text{ A}}{\pi \cdot (1.00 \times 10^{-3}\text{ m}) \cdot (4.60 \times 10^{-6}\text{ V})} \approx 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}

    You repeated the unit conversion omission by substituting 4.604.60 instead of 4.60×10−6 V4.60 \times 10^{-6}\text{ V}, which gave a value 10610^6 times too small.

  4. Step 4

    Specimen 1 has highest conductivity so it is Ag. Specimen 3 has intermediate conductivity so it is Cu. Specimen 2 has lowest conductivity so it is Pb. Specimen 2 tarnishes because lead oxidizes in air to form a dull lead oxide coating.

WHAT YOU DID WELL
Compliments from Your Teacher

You algebraically set up the relationship between bulk conductivity, sheet resistance, and four-point probe parameters correctly.

You converted current and thickness into proper base SI units (0.100 A0.100\text{ A} and 0.001 m0.001\text{ m}).

You accurately ranked the conductivities to identify Silver, Copper, and Lead.

You correctly explained that lead's loss of luster is caused by the formation of an oxide layer.

THE ERROR
Where Your ACEpath Teacher Spotted the Mistake
Missing SI prefix conversion

You treated microvolts directly as volts during numerical substitution.

WHY IT HAPPENED
ACEpath Teacher's Diagnosis

You overlooked the metric prefix μ\mu (10−610^{-6}) when moving from the given experimental data to the formula substitution, leading to calculated values that were off by six orders of magnitude.

REASONING PATH
Your ACEpath teacher’s suggested approach
SI Prefix Verification
  • 1 μV=10−6 V1\ \mu\text{V} = 10^{-6}\text{ V}

  • Always write out each given quantity in scientific notation with base SI units before substituting into physical equations.

Physical Reality Check for Metals
  • Good conductors like Ag\ce{Ag} and Cu\ce{Cu} have electrical conductivities on the order of 107 Ω−1⋅m−110^7\ \Omega^{-1}\cdot\text{m}^{-1}.

  • Compare calculated values against typical reference scales: a value of ∼60 S/m\sim 60\text{ S/m} corresponds to poorly conducting electrolytes, not metallic conductors.

CORRECTED PATH
ACEpath Teacher's Demonstration
  1. Convert measured voltage drops from microvolts to volts: ΔV1=0.350 μV=0.350×10−6 V\Delta V_1 = 0.350\ \mu\text{V} = 0.350 \times 10^{-6}\text{ V} and ΔV2=4.60 μV=4.60×10−6 V\Delta V_2 = 4.60\ \mu\text{V} = 4.60 \times 10^{-6}\text{ V}.

  2. Evaluate σ1=ln⁡(2)⋅0.100 Aπ⋅(1.00×10−3 m)⋅(0.350×10−6 V)=6.30×107 Ω−1⋅m−1\sigma_1 = \frac{\ln(2) \cdot 0.100\text{ A}}{\pi \cdot (1.00 \times 10^{-3}\text{ m}) \cdot (0.350 \times 10^{-6}\text{ V})} = 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}.

  3. Evaluate σ2=ln⁡(2)⋅0.100 Aπ⋅(1.00×10−3 m)⋅(4.60×10−6 V)=4.80×106 Ω−1⋅m−1\sigma_2 = \frac{\ln(2) \cdot 0.100\text{ A}}{\pi \cdot (1.00 \times 10^{-3}\text{ m}) \cdot (4.60 \times 10^{-6}\text{ V})} = 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}.

Final answer

(a) Specimen 1: σ1=6.30×107 Ω−1⋅m−1\sigma_1 = 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}; Specimen 2: σ2=4.80×106 Ω−1⋅m−1\sigma_2 = 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}. (b) Specimen 1 is Ag\ce{Ag}, Specimen 2 is Pb\ce{Pb}, Specimen 3 is Cu\ce{Cu}; Specimen 2 tarnishes because spontaneous oxidation in air produces a non-metallic PbO\ce{PbO} coating that diffusely scatters light.

NEXT STEPS
Final Takeaways from Your Teacher
  • Practice converting metric prefixes (such as μ\mu, m\text{m}, and k\text{k}) immediately in your given-data list before touching the calculator.

  • Check that your final numerical values match the expected physical magnitude for the material class you are evaluating.

OverviewACEpath Teacher's Diagnosis

02 The student misinterprets higher measured voltage as indicating higher conductivity rather than higher resistance, reversing the metal assignments.

Sample Student Work

Reviewed by ACEpath Teacher
Step-by-Step Review
Walk Through It with Your Teacher
Partially correct
  1. Step 1

    σ=ln⁡(2)⋅Iπ⋅t⋅ΔV  ⟹  σ1=ln⁡(2)⋅0.100π⋅1.00×10−3⋅0.350×10−6=6.30×107 S/m  ⟹  σ2=ln⁡(2)⋅0.100π⋅1.00×10−3⋅4.60×10−6=4.80×106 S/m\sigma = \frac{\ln(2) \cdot I}{\pi \cdot t \cdot \Delta V} \implies \sigma_1 = \frac{\ln(2) \cdot 0.100}{\pi \cdot 1.00 \times 10^{-3} \cdot 0.350 \times 10^{-6}} = 6.30 \times 10^7\text{ S/m} \implies \sigma_2 = \frac{\ln(2) \cdot 0.100}{\pi \cdot 1.00 \times 10^{-3} \cdot 4.60 \times 10^{-6}} = 4.80 \times 10^6\text{ S/m}

  2. Step 2

    Higher voltage drop means higher conductivity. Specimen 2 has the largest ΔV=4.60 μV\Delta V = 4.60\ \mu\text{V}, so Specimen 2 is Ag\ce{Ag}. Specimen 3 has ΔV=0.372 μV\Delta V = 0.372\ \mu\text{V}, so Specimen 3 is Cu\ce{Cu}. Specimen 1 has the lowest ΔV=0.350 μV\Delta V = 0.350\ \mu\text{V}, so Specimen 1 is Pb\ce{Pb}.

    Correct

    Because σ∝1ΔV\sigma \propto \frac{1}{\Delta V} at constant current and geometry, a lower potential difference indicates higher electrical conductivity. Since intrinsic conductivity follows σ(Ag)>σ(Cu)>σ(Pb)\sigma(\ce{Ag}) > \sigma(\ce{Cu}) > \sigma(\ce{Pb}), Specimen 1 (lowest ΔV\Delta V, highest σ\sigma) is Ag\ce{Ag}, Specimen 3 is Cu\ce{Cu}, and Specimen 2 (highest ΔV\Delta V, lowest σ\sigma) is Pb\ce{Pb}.

    You inverted the relationship between voltage drop and conductivity. From Ohm's law, a larger potential drop ΔV\Delta V across a given current indicates greater resistance, which means lower conductivity.

  3. Step 3

    Specimen 2 loses luster due to surface reaction forming an oxide layer.

    Correct

    Lead (Specimen 2) loses its metallic luster because spontaneous reaction with atmospheric OX2\ce{O2} and COX2\ce{CO2} forms an incoherent, non-metallic PbO\ce{PbO}/PbCOX3\ce{PbCO3} surface film that causes diffuse scattering of incident light rather than specular reflection.

    You correctly recognized that tarnishing is caused by a surface reaction forming an oxide layer, but this explanation applies chemically to Lead (Pb\ce{Pb}), not Silver (Ag\ce{Ag}).

WHAT YOU DID WELL
Compliments from Your Teacher

You derived and correctly set up the reciprocal relationship for conductivity from sheet resistance.

You accurately carried out the numerical calculations for both specimens with correct scientific notation and units.

You identified that oxidation reactions at the metal surface cause tarnishing.

THE ERROR
Where Your ACEpath Teacher Spotted the Mistake
Inverted proportionality between voltage drop and conductivity

none

WHY IT HAPPENED
ACEpath Teacher's Diagnosis

You treated measured voltage drop as directly proportional to electrical conductivity instead of inversely proportional to it, overlooking that for a fixed test current, ΔV=IR\Delta V = I R means higher ΔV\Delta V corresponds to greater resistance and lower conductivity.

REASONING PATH
Your ACEpath teacher’s suggested approach
Voltage-Conductivity Relationship
  • For a constant current II, ΔV=IR∝1σ\Delta V = I R \propto \frac{1}{\sigma}.

  • Always associate a larger voltage drop with higher electrical resistance and lower conductivity.

Intrinsic Metal Conductivity Ranking
  • Among common conductive metals, conductivity decreases in the order Ag>Cu>Au>Al>⋯>Pb\ce{Ag} > \ce{Cu} > \ce{Au} > \ce{Al} > \dots > \ce{Pb}.

  • Assign the metal with the smallest measured ΔV\Delta V to the most conductive metal (Silver).

CORRECTED PATH
ACEpath Teacher's Demonstration
  1. Recall that σ=ln⁡(2)IπtΔV\sigma = \frac{\ln(2) I}{\pi t \Delta V}, which shows that σ\sigma is inversely proportional to ΔV\Delta V.

  2. Rank the specimens by conductivity: Specimen 1 (ΔV=0.350 μV\Delta V = 0.350\ \mu\text{V}, highest σ\sigma) > Specimen 3 (ΔV=0.372 μV\Delta V = 0.372\ \mu\text{V}) > Specimen 2 (ΔV=4.60 μV\Delta V = 4.60\ \mu\text{V}, lowest σ\sigma).

  3. Match with the known conductivity trend σ(Ag)>σ(Cu)>σ(Pb)\sigma(\ce{Ag}) > \sigma(\ce{Cu}) > \sigma(\ce{Pb}) to identify Specimen 1 as Ag\ce{Ag}, Specimen 3 as Cu\ce{Cu}, and Specimen 2 as Pb\ce{Pb}.

  4. Explain that Pb\ce{Pb} spontaneously oxidizes in air to form an amorphous/microcrystalline PbO/PbCOX3\ce{PbO}/\ce{PbCO3} layer lacking free conduction electrons, converting specular reflection into diffuse scattering.

Final answer

(a) Specimen 1: σ=6.30×107 Ω−1⋅m−1\sigma = 6.30 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}; Specimen 2: σ=4.80×106 Ω−1⋅m−1\sigma = 4.80 \times 10^6\ \Omega^{-1}\cdot\text{m}^{-1}. (b) Specimen 1 is Ag\ce{Ag}, Specimen 2 is Pb\ce{Pb}, and Specimen 3 is Cu\ce{Cu}; Lead loses luster because a non-conductive surface layer of PbO/PbCOX3\ce{PbO}/\ce{PbCO3} forms and scatters light diffusely rather than specularly.

NEXT STEPS
Final Takeaways from Your Teacher
  • Check algebraic formulas for inverse relationships before drawing qualitative conclusions from data.

  • Review how Ohm's law (V=IRV = IR) relates voltage drop across conductors to their resistance and conductance.

  • Connect metallic luster to the sea-of-electrons model: free valence electrons produce specular reflection, whereas ionic/covalent corrosion products produce diffuse scattering.

Lock it in

Similar question

01

A copper wire with cross-sectional area A=2.00 mm2A = 2.00\text{ mm}^2 and length L=5.00 mL = 5.00\text{ m} carries a current of 2.00 A2.00\text{ A} with an observed voltage drop of ΔV=84.0 μV\Delta V = 84.0\ \mu\text{V}. Calculate the electrical conductivity σ\sigma of the wire in Ω−1⋅m−1\Omega^{-1}\cdot\text{m}^{-1}.

Answer

σ=5.95×107 Ω−1⋅m−1\sigma = 5.95 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}. Convert units: A=2.00×10−6 m2A = 2.00 \times 10^{-6}\text{ m}^2 and ΔV=8.40×10−5 V\Delta V = 8.40 \times 10^{-5}\text{ V}. Using R=ΔVI=8.40×10−5 V2.00 A=4.20×10−5 ΩR = \frac{\Delta V}{I} = \frac{8.40 \times 10^{-5}\text{ V}}{2.00\text{ A}} = 4.20 \times 10^{-5}\ \Omega, then σ=LR⋅A=5.00(4.20×10−5)(2.00×10−6)=5.95×107 Ω−1⋅m−1\sigma = \frac{L}{R \cdot A} = \frac{5.00}{(4.20 \times 10^{-5})(2.00 \times 10^{-6})} = 5.95 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}.

02

An aluminum thin film of thickness t=500 nmt = 500\text{ nm} is measured with a collinear four-point probe (Rs=πln⁡(2)ΔVIR_s = \frac{\pi}{\ln(2)}\frac{\Delta V}{I}). At I=10.0 mAI = 10.0\text{ mA}, the recorded voltage is ΔV=16.5 μV\Delta V = 16.5\ \mu\text{V}. Determine (a) the sheet resistance RsR_s and (b) the bulk electrical conductivity σ\sigma.

Answer

(a) Rs=7.48×10−3 Ω/□R_s = 7.48 \times 10^{-3}\ \Omega/\Box; (b) σ=2.67×107 Ω−1⋅m−1\sigma = 2.67 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}. Convert I=0.0100 AI = 0.0100\text{ A}, ΔV=1.65×10−5 V\Delta V = 1.65 \times 10^{-5}\text{ V}, and t=5.00×10−7 mt = 5.00 \times 10^{-7}\text{ m}. Calculate Rs=πln⁡(2)⋅1.65×10−50.0100≈7.478×10−3 ΩR_s = \frac{\pi}{\ln(2)} \cdot \frac{1.65 \times 10^{-5}}{0.0100} \approx 7.478 \times 10^{-3}\ \Omega. Then σ=1Rs⋅t=1(7.478×10−3)(5.00×10−7)=2.67×107 Ω−1⋅m−1\sigma = \frac{1}{R_s \cdot t} = \frac{1}{(7.478 \times 10^{-3})(5.00 \times 10^{-7})} = 2.67 \times 10^7\ \Omega^{-1}\cdot\text{m}^{-1}.

03

Two metallic specimens, A and B, are tested. Specimen A maintains a specular gloss of 94 GU94\text{ GU} after prolonged air exposure and exhibits conductivity σ=6.20×107 S/m\sigma = 6.20 \times 10^7\text{ S/m}. Specimen B initially has 92 GU92\text{ GU} but drops to 18 GU18\text{ GU} over 48 hours, with conductivity σ=4.80×106 S/m\sigma = 4.80 \times 10^6\text{ S/m}. Identify which metal is Lead (Pb) and which is Silver (Ag), and contrast the microscopic optical behavior of their surfaces after 48 hours.

Answer

Specimen A is Silver (Ag); Specimen B is Lead (Pb). Silver resists rapid spontaneous oxidation in clean air, maintaining an unoxidized electron-sea surface that produces specular (mirror-like) light reflection (94 GU94\text{ GU}). Lead rapidly reacts with atmospheric OX2\ce{O2} and COX2\ce{CO2} to form an irregular, non-metallic PbO/PbCOX3\ce{PbO}/\ce{PbCO3} layer that diffusely scatters incoming light in all directions, dropping gloss to 18 GU18\text{ GU}.